This study presents a fused deposition modeling‐based method for fabricating resin‐bonded diamond grinding wheels to address limitations of conventional microwheel manufacturing, including low material utilization, high equipment cost, and demanding mold precision. Molecular dynamics simulations and finite element analysis were combined to investigate the rheological behavior of acrylonitrile butadiene styrene (ABS)/polyvinyl chloride (PVC)/diamond abrasive /dioctyl phthalate (DOP) composites and optimize five resin‐bonded diamond composite (RDC) formulations (RDC1–RDC5). A thermo‐mechanical model of the nozzle flow channel and grinding wheel was established in Ansys Workbench to analyze temperature, viscosity, velocity, stress, and strain distributions. Results show that DOP improves melt flowability by reducing polymer‐chain entanglement and interfacial friction. Experimental validation demonstrates that a 0.1 mm layer thickness and 30 mm/s printing speed effectively reduce thermal stress and strain, while a 1.25 mm wall thickness promotes structural densification. Surface morphology confirms that 0.1 mm layers are free of visible microdefects, whereas larger layer thicknesses (0.15–0.2 mm) produce interlayer defects. These findings provide optimized processing parameters and a theoretical basis for high‐precision, low‐cost additive manufacturing of micro diamond grinding wheels for hard and brittle material machining.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: