This article reviews the effects of applied bias and temperature on Si/SiO2interface-trap buildup and annealing rates. Electrical and spectroscopic methods are described to estimate interface-trap densities at oxidized Si surfaces, in MOS capacitors and transistors, and in linear bipolar devices. Illustrative results provide insights into the kinetics and energetics of interface-trap annealing. Interface traps in MOS and linear bipolar devices anneal much more easily at 0 V bias than at positive or negative applied bias. Hydrogen transport and reactions play critical roles in interface-trap buildup and annealing processes. The complex interplay between H2diffusion and H+drift is illustrated via coupled experimental and theoretical studies. Interface-trap annealing imposes significant constraints on hardness-assurance techniques. Current MOS standard tests that incorporate accelerated aging at elevated temperature at worst case, static, positive bias enable successful assessment of MOS devices in low-dose-rate environments. However, it is not similarly possible to use elevated-temperature irradiation and/or annealing at worst case, 0 V bias to predict low-dose-rate response for linear bipolar devices and ICs. Temperature-switching during irradiation appears to be a promising approach to address this issue.
No takes yet. Share an insight, caveat, or question.
Daniel M. Fleetwood (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: