Answers are grounded in this paper and cite their sources.
The epitaxial quality of GexSi1−x films grown on Si〈100〉 by a novel laser-assisted technique has been investigated for compositions in the range x≤0.37 and thicknesses between 50 and 500 nm. Epitaxy is induced during electron beam deposition of GexSi1−x films on Si substrates by pulses of an excimer laser operating at 308 nm with 30 ns pulse duration. Good epitaxial growth is obtained for 50 nm films for x≤0.04 on chemically cleaned Si(100) surfaces even in the presence of substantial fluorine coverage. Using a predeposition/crystallization of a 50 nm pure-Si buffer layer, good epitaxy is then obtained in 50 nm films for x=0.05–0.13. At x=0.07, defect-free alloys have been grown up to thicknesses of 0.5 μm. However, for films with compositions above 19 at.% Ge, dislocations at a nearly constant density of ≊10 μm/μm2 are observed. This uniform density suggests a breakdown mechanism other than simple strain relaxation.
No takes yet. Share an insight, caveat, or question.
Lombardo et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: