Answers are grounded in this paper and cite their sources.
In this research study, mild steel adherends were bonded using unreinforced and titanium dioxide (TiO 2 ) nanoparticle‐reinforced adhesives (1.0 wt%, 2.0 wt%, 3.0 wt%, and 4.0 wt%) to form single‐lap joints. The adhesive joints were exposed to hygrothermal aging for 1, 2, 3, and 4 weeks. Lap shear tests revealed that the mean shear strength of unreinforced adhesive joints was 10.627 MPa, and with reinforcement, the shear strength increased by up to 54% in unaged conditions. After 4 weeks of aging, shear strength reductions were observed, with unreinforced joints experiencing a 66% loss, while 3.0 wt% reinforced joints exhibited the lowest reduction at only 13%, demonstrating their effectiveness in maintaining adhesive strength. Water absorption was significantly reduced by up to 56% with reinforcement, minimizing moisture‐induced degradation. Contact angle measurements showed an increase in surface hydrophobicity, with the 3.0 wt% reinforced adhesive reaching the highest contact angle of 89° ± 2°. Differential Scanning Calorimetry (DSC) analysis confirmed changes in glass transition temperature ( T g ) due to aging. High‐resolution (HRSEM) analysis revealed morphological changes and crack formations, highlighting the impact of hygrothermal aging on adhesive joint durability.
No takes yet. Share an insight, caveat, or question.
Pragathi et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: