Answers are grounded in this paper and cite their sources.
A polycrystalline silicon film 0.55 μm thick was deposited in a low-pressure CVD reactor on a Si3N4 substrate. Islands of various sizes (2×20 μm up to 20×160 μm) were prepared by standard photolithographic techniques. Laser annealing was then performed under conditions which are known to cause an increase in grain size from ∼500 Å to long narrow crystals of 2×25 μm in a continuous polysilicon film. These same conditions were found to produce single-crystal 〈100〉 material in the (2×20 μm) islands. However, 25×25-μm and 20×160-μm islands remain polycrystalline after the laser scan.
No takes yet. Share an insight, caveat, or question.
Gibbons et al. (1979) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: